SBDs fabricated on annealed (at 450°C for 30 minutes) He-processed samples exhibited improved but still poor rectification. In contrast, SBDs fabricated on annealed SiCl 4 etched surfaces had virtually the same characteristics as those fabricated on unannealed SiCl 4 etched samples.